Micro injection molding has become a cornerstone for mass-producing microfluidic devices, yet demolding defects and mold wear remain persistent challenges. This study introduces a nickel mold ...
Porous rods of poly(tetrafluoroethylene) (PTFE) were fabricated by molding PTFE powder and fumaric acid (FA) at room temperature and sintering at 400 °C. The ...